花紋鋁板染色需要注意哪些問題?

來源:http://www.kwcwb.cn/ 發(fā)布時(shí)間:2023-12-28

鋁板廠是如何解決花紋鋁板染色問題,花紋鋁板因其裝飾性耐用性等優(yōu)良特性,廣受市民青睞,可是在生產(chǎn)過程中有一些花紋鋁板的染色問題,不能達(dá)到生產(chǎn)商的期望的效果,為了解決這一問題,鋁板廠為大家分享四種解決花紋鋁板染色問題的辦法。

How does the aluminum plate factory solve the dyeing problem of patterned aluminum plates? Patterned aluminum plates are widely favored by citizens due to their excellent characteristics such as decoration, durability, etc. However, there are some dyeing problems in the production process of patterned aluminum plates that cannot meet the expected results of the manufacturer. To solve this problem, the aluminum plate factory shares four methods to solve the dyeing problem of patterned aluminum plates.

選擇好的鋁板制件原料:通常生產(chǎn)過程中的高純鋁鋁鎂鋁錳合金經(jīng)過陽極氧化以后,其染色的功能是好的,可以染成各種各樣的顏色。對(duì)于含硅或銅比較重的板材,在染色的過程中只能夠染成深色與黑色,比較單調(diào)的顏色。

Choose the right raw materials for aluminum plate parts: usually, high-purity aluminum aluminum magnesium aluminum manganese alloy in the production process is anodized, and its dyeing function is good, which can be dyed into various colors. For boards with heavy silicon or copper content, only dark and black colors can be dyed during the dyeing process, which are relatively monotonous.

20230708124018625.jpg

控制好氧化膜的厚度:氧化膜就是指鋁板膜層的厚度孔隙率透明度等。鋁板中膜層的厚度保持在10um以上就可以了,孔隙率以及透明度,可以得到好的染色質(zhì)量。

Control the thickness of the oxide film: The oxide film refers to the thickness, porosity, transparency, etc. of the aluminum plate film layer. The thickness of the film layer in the aluminum plate should be maintained above 10um, and the porosity and transparency can achieve good dyeing quality.

把握好染色液的濃度:鋁板的濃度與染色之間有著聯(lián)系,如果鋁板染淡色,其中濃度可以低一點(diǎn),染深色其濃度可以高一點(diǎn)。通常所生產(chǎn)的鋁板材料所染比較淡的顏色其色彩為0。1-0。39g/L,染淡色彩為1g/L,染深色彩為3-5g/L,染稠密的色彩為10-15g/L,如果染色的濃度比較高就會(huì)造成顏色不均或出現(xiàn)浮色現(xiàn)象,在清潔與關(guān)閉的過程中容易出現(xiàn)“流色”。為了加強(qiáng)染色的吸附性,會(huì)使用低濃度顏色進(jìn)行延伸染色,這樣可以使染料分子比較均勻的滲透到氧化膜孔隙的深處,這樣可以使所染的顏色更加和諧與牢固。

Grasp the concentration of the dyeing solution: There is a connection between the concentration of aluminum plate and dyeing. If the aluminum plate is dyed light, the concentration can be lower, and if dyed dark, the concentration can be higher. The color of the aluminum plate material that is usually dyed lighter is 0. 1-0. 39g/L, light color is 1g/L, deep color is 3-5g/L, and dense color is 10-15g/L. If the dyeing concentration is relatively high, it will cause uneven color or floating color phenomenon, which is easy to occur during the cleaning and closing process. In order to enhance the adsorption of dyeing, low concentration colors are used for extended dyeing, which can allow dye molecules to penetrate more evenly into the deep pores of the oxide film, making the dyed color more harmonious and firm.

控制好染色液溫度:鋁板的染色分為冷染與熱染。使用冷染,在生產(chǎn)的過程中使用的時(shí)間比較長,所染色彩均勻性比較好掌握。熱染使用的時(shí)間比較短,但是對(duì)顏色的操控比較難。熱染的溫度在通常在40-60℃。如果溫度過高,會(huì)減小染色的吸附性,并且容易導(dǎo)致鋁板的表面發(fā)花。

Control the temperature of the dyeing solution: The dyeing of aluminum plates is divided into cold dyeing and hot dyeing. Cold dyeing is used for a relatively long time during the production process, and the uniformity of the dyed color is easy to control. The use time of hot dyeing is relatively short, but it is difficult to control the color. The temperature of hot dyeing is usually between 40-60 ℃. If the temperature is too high, it will reduce the adsorption of dyeing and easily cause the surface of the aluminum plate to flower.